TPS-DSC-OM4 Differential Scanning Calorimeter
Summary:
One-key operation, automatic operation, isothermal Oxidative induction time special equipment
The DSC is a touch screen type, specially testing polymer material oxidation induction period test, customer one-key operation, software automatic operation.
Support one experiment to measure 4 samples
Conforming the following standards:
GB/T 19466.6- 2009/ISO 11357-3:1999 No.6
Features:
l Industrial level widescreen touch structure is rich in information, including setting temperature, sample temperature, oxygen flow, nitrogen flow, differential thermal signal, various switch states, etc.
l Support to measure two samples at the same time, the efficiency is greatly improved by 2 times. It is very convenient to measure multiple samples at the same furnace body at the same time. If we make 5 sample data in strict accordance with the requirements of national standard, we can finish the data quantity measured in 1 day instead of 2 days. It can not only save time, but also ensure the uniformity of data measurement conditions and quickly judge the sample uniformity.
l New imported sensor sample bracket, fully closed structure design, prevent items from falling into the furnace body.
l USB communication interface, strong universality, reliable communication, support self-restoring connection function.
l The furnace structure is compact, and the rate of rising and cooling is adjustable.
l The installation process is improved, and the mechanical fixation method is adopted to completely avoid the contamination of the internal colloidal of the furnace to the differential heat signal.
l The furnace is heated by heating wire, compact structure and small size.
l The double temperature probe ensures the high repeatability of the sample temperature measurement, and adopts the special temperature control technology to control the temperature of the furnace wall to set the temperature of the sample.
l The gas flow meter automatically switches between two channels of gas, with fast switching speed and short stable time.
l Standard sample is provided for easy adjustment of temperature coefficient.
l Software support each resolution screen, automatically adjust the computer screen size curve display mode. Support laptop, desktop; Support Win2000, XP, VISTA, WIN7, WIN8, WIN10 and other operating systems.
l Support user edit device operation mode according to actual needs to achieve full automation of measurement steps. The software provides dozens of instructions, and users can flexibly combine and save each instruction according to their own measurement steps. Complex operations are reduced to one-click operations.
Parameters:
1. Temperature range: RT-500℃
2. Temperature resolution:0.01℃
3. Heating rate: 0.1~80℃/min
4. Cooling rate: 0.1~30℃/min
5. Constant temperature: RT-500℃
6. Duration of constant temperature: The duration is recommended to be less than 24 hours.
7. Temperature control mode: Constant temperature rise, constant temperature
8. Quantity of samples for a single test: 4 samples at a time
9. DSC range: 0~±500mW
10. DSC resolution: 0.01mW
11. DSC sensitivity: 0.01mW
12. Working power: AC 220V 50Hz 300W or other
13. Atmosphere control gas: Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen)
14. Gas flow:0-200mL/min
15. Gas pressure:0.2MPa
16. Gas flow accuracy: 0.2mL/min
17. Crucible: Aluminium crucible Φ6.6*3mm (Diameter * High)
18. Calibration standard: with standard material (indium, tin, zinc), users can adjust the temperature coefficient by themselves
19. Data interface: Standard USB interface
20. Display mode: 7-inch touch screen
21. Output mode: computer and printer
22. Fully closed support structure design, prevent items falling into the furnace body, pollution of the furnace body, reduce the maintenance rate